Super Duplex S32760/ F55, Super Duplex Alloy UNS S32760 (F55 / 1.4501) gen ekselan rezistans Pitting ak Kowozyon Crevice nan dlo lanmè nan tanperati ki wo, apwovizyone ak yon PREN 40<( Pitting Resistance Eqv).Ekselan rezistans nan SCC (Stress Kowozyon Cracking) nan anviwònman tounen ak klori.
● UNS S32750, F53● ASTM A 240, A790, A815, A182, A 276, A 476, A789● EN 1.4410● Lòt non komen SAF 2507®